INCONEL® qotishmasi C-276 UNS N10276/W.Nr. 2.4819
Qotishma | element | C | Si | Mn | S | P | Ni | Cr | Mo | W | Fe | Co | V |
QotishmaC-276 | Min | 14.5 | 15.0 | 3.0 | 4.0 | ||||||||
Maks | 0,01 | 0,08 | 1.0 | 0,03 | 0,04 | Balanga | 16.5 | 17.0 | 4.15 | 7.0 | 2.50 | 0,35 |
Aolly holati | Mustahkamlik chegarasi Rm Mpa Min | Hosildorlik kuchi RP 0. 2Mpa Min | Cho'zilish A 5% Min |
Solutsiya | 690 | 283 | 45 |
Zichlikg/sm3 | Erish nuqtasi℃ |
8.89 | 1325~1370 |
Rod, bar, sim va zarb zahiralari -ASTM B 462 (tayoq, bar va zarb zaxirasi), ASTM B 564 va, ASTM B 574 (sim)
Plita, varaq va tasma- ASTM B 575/B 906 va ASME SB 575/SB 906
Quvur va quvur -ASTM B 622/B 829 va ASME SB 622/SB 829 (choksiz quvur), ASTM B 626/B 751 va ASME SB 626/SB751 (payvandlangan quvur), ASTM B 619/B 775
Payvandlash mahsulotlari -INCONEL to'ldiruvchi metall C-276 - AWS A5.14 / ERNiCrMo-4.
2000 yilgacha ajoyib oksidlanish qarshiligi° F
● Karbürizatsiya va nitridlanishga chidamli
● Zo'r yuqori harorat kuchi
● Xlorid stress-korroziya yorilishiga yaxshi qarshilik